大直径薄壁TC4钛合金无缝管的热扩管工艺研究

    Research on Hot-expansion Process for Large-sized Light-wall TC4 Titanium Alloy Seamless Tube

    • 摘要: 针对大直径薄壁钛合金无缝管热轧温降快、成材率低难题,借助有限元方法对TC4钛合金无缝管的热扩管过程进行模拟,采用Gleeble试验机开展短时高温氧化-拉伸试验,研究TC4钛合金无缝管在热扩过程中的壁厚偏差变化规律以及扩管温度对管材表面质量和显微组织的影响。发现同轴度偏差管坯扩管后偏心程度会增加8%,圆柱度偏差增加15%,圆柱度偏差管坯扩后的壁厚偏心率增加27.9%,同轴度偏差管坯扩后的外壁离心率从0增加到15.7%。随着扩管管坯加热温度的升高,TC4钛合金管的组织从相对离散的颗粒状逐渐向细长的针状转变,并细化增多形成更为复杂的网络状或交织状组织,表面氧化层的开裂程度增加,最大深度达到20μm。

       

      Abstract: Addressing the problems of rapid temperature loss and low yield as met during the hot rolling of the large-sized, light-walled seamless titanium alloy tube, the hot-expansion process of the TC4 titanium alloy seamless tube is simulated with the finite element method. And the Gleeble simulator is used to conduct the short-time hi-temperature oxidation-tensile test so as to research the regularity of W.T. deviation changes of the said tube during the hot-expansion process as well as the effect of the hot-expansion temperature on the surface quality and the microstructure of the tube. It is revealed via the study that for the mother tube with coaxiality deviation, its eccentricity is increased by 8% after expansion,and its cylindricity deviation is increased by 15%. As for the mother tube with cylindricity deviation,its post-expansion W.T. eccentricity is increased by 27.9%,while outer wall eccentricity of the mother tube with coaxiality deviation is increased from 0 to 15.7%. Along with rise of the heating temperature of the mother tube,the microstructure of TC4 the titanium alloy tube is gradually transformed from relatively discrete granular particles to elongated needle-like structures, and becomes finer and grows to form a more complex network or interwoven structure, leading to the further cracking of the surface oxidation layer with maximum depth up to 20 μm.

       

    /

    返回文章
    返回