14MnVNb无缝钢管外折缺陷产生原因分析

    Analysis on Causes for Outer Fold Defect of 14MnVNb Seamless Steel Pipe

    • 摘要: 针对14MnVNb连铸坯轧制X60Q管线管出现的外折缺陷,分析缺陷产生原因并提出改进措施。结果表明:外折缺陷源于连铸坯表面的横裂纹;连铸机活动段喷嘴漏水、密封圈高温失效,造成连铸坯局部冷却不均,进入拉矫机时温度偏低,使得连铸坯表面产生横裂纹。通过将喷嘴氟胶密封圈改为金属密封圈,降低二冷比水量至0.15 L/kg,提高拉坯速度至0.30 m/min等,可使连铸坯进入拉矫机时温度提升至882℃,无缝钢管超声波探伤合格率由81.93%提高至93.75%。研究揭示了连铸坯进入拉矫机温度对连铸坯表面裂纹的影响机制,为同类钢管外折的防控提供了工程参考。

       

      Abstract: Addressing the outer fold defect as occurring in the X60Q pipeline steel pipe rolled from the 14 Mn VNb CC billet, the causes of the defect are identified via relevant analysis, and then improvement measures are proposed.The analysis result shows that the outer fold defect is originated by the surface transverse cracks of the CC billet. And the said cracks are caused by a number of factors,including the nozzle leakage in the moving section of the continuous casting machine,and the high-temperature failure of the sealing ring,which leads to uneven local cooling of the billet and a low temperature of the billet at the inlet of the straightening machine. Accordingly countermeasures are taken, including substituting the nozzle metal sealing ring for the fluorine rubber sealing ring,reducing the secondary cooling specific water rate to 0.15 L/kg and increasing the CCM withdraw speed to 0.30 m/min. As a result the CC billet temperature at the straightening inlet is raised to 882 ℃,and the ultrasonic testing qualification rate is increased from 81.93% to 93.75%. The above mentioned study reveals the mechanism of influence on the occurrence of the CC billet surface crack by the CC billet temperature at the straightening machine inlet,providing an engineering reference for preventive control of similar outer fold defect of the steel pipe.

       

    /

    返回文章
    返回