Gr.6无缝钢管低温冲击韧性异常波动原因分析

    Analysis of Abnormal Fluctuation of Low-temperature Impact Toughness of Gr.6 Seamless Steel Pipe

    • 摘要: Gr.6无缝钢管长期服役于低温环境,低温韧性直接影响其使用寿命和安全性能。针对某批次Gr.6无缝钢管-45℃冲击功异常波动的问题,对冲击功异常试样的夹杂物、室温组织特征以及断口形貌进行表征分析。结果表明,带状组织和大小角度晶界分布不均匀是导致Gr.6无缝钢管低温冲击韧性异常波动的主要原因。建议热处理时加快冷却速度,严格控制加热时间和温度,以减少带状组织,提高组织均匀性,确保产品质量。

       

      Abstract: Due to long-term service in low-temperature environment,the service span and safety performance of the Gr.6 seamless steel pipe is directly affected by the low temperature toughness. Addressing a certain batch of the Gr.6 seamless steel pipe with abnormal fluctuation of-45 ℃ impact energy,characterization analyses are conducted on the inclusion,the room temperature microstructure characteristics and the post-fracture morphology. As a result it is identified that the banded structure and the uneven distributions of high-angle and low-angle grain boundaries act as the main cause for the abnormal fluctuation of the said Gr.6 pipe. Accordingly, it is suggested to enhance the cooling rate during the heat treatment,and strictly control the heating time and temperature to reduce the banded structure and enhance the structural homogeneity so as to assure of the product quality.

       

    /

    返回文章
    返回