热轧20G减径厚壁钢管压扁工艺性能不稳定原因及改进措施

    CAUSE-ANALYSIS OF ANTI-FLATTENING PROPERTY NON-CONSISTENCE OF HOT ROLLED/REDUCED HEAVY-WALLED 20G STEEL PIPE AND RELEVANT IMPROVEMENT MEASURES

    • 摘要: 分析了上钢一厂热轧20G减径厚壁管压扁工艺性能不稳定的原因。增加正火工艺,改钢管热轧状态交货为热处理状态交货,其压扁工艺性能不稳定明显改善。

       

      Abstract: Factors responsible for the anti-flattening pioperty non-consistence of hot rolled/reduced heavy-walled 20G steel pipe made by Shanghai No.1 I & S Works are analyzed. Accordingly relevant impiovement measures are established, including addition of normalization treatment, changing the pipe delivery condition from being hot-rolled into being heat treated etc., which enable a significant improve-ment of the said non-consistence.

       

    /