    • 摘要: 采用慢应变速率拉伸法,通过扫描电镜、能谱分析等手段,分析不同温度和干/湿气环境(通入H2和CO2混合气体)下HP13Cr、13Cr、3Cr的氢脆敏感性。结果显示:干气环境下,温度对这3种材质氢脆敏感性的影响较小;120℃干气环境中的氢脆系数排序为HP13Cr<13Cr<3Cr;湿气环境中,由于Cl-和CO2水溶液的综合作用,13Cr氢脆系数增大,但不同试验条件下的氢脆系数均未大于25%,可以认为其并无氢脆敏感性倾向。针对模拟的含氢储气库试验条件,推荐使用13Cr系列材质。

       

      Abstract: Analyzed is the hydrogen-embrittlement sensitivity of the HP13Cr, 13Cr and 3Cr pipes presented under the conditions of different temperatures and dry/humid gas(H2 and CO2 combination)environment by means of the SSRT method, and the scanning electron microscope(SEM)and the energy dispersive X-ray spectrometer(EDS).The testing result reveals the facts as follows.In the dry gas environment, the temperature produces little effect on the sensitivities of the said three different pipes, while in the 120℃ dry gas environment, the sequence of hydrogenembrittlement sensitivity coefficients of the said pipes is HP13Cr<13Cr<3Cr;And in the humid gas environment, due to the combined effects by the Cl-concentration and the CO2 water solution, the hydrogen embrittlement coefficient of the 13Cr pipe is increased, but in case of any testing conditions, none of the said coefficients has got higher than 25%, which can be interpreted as no trend of hydrogen-embrittlement exists.Based on the simulated testing conditions of the hydrogen-containing gas storage, the 13Cr series tubular material is recommended for actual applications.

       

    /

    返回文章
    返回