42CrMo钢芯棒开裂的失效分析

    INVESTIGATION OF CRACK-CAUSED OUT-OF-WORK 42CrMo STEEL MANDREL

    • 摘要: 42CrMo钢芯棒在感应淬火及回火后表面出现环向裂纹,通过对其裂纹部位的组织等进行宏观、低倍及高倍观察和分析,找出了环向裂纹产生的原因。

       

      Abstract: Circular cracks developed on the surface of the 42CrMo steel mandrel after induction quenching/tempering. With the macro and micro analysis of the crack area's structure, the causes responsible for the said cracks have been found.

       

    /