中小直缝焊管内焊筋缺陷成因及其预防措施

    INVESTIGATION OF ELEMENTS RESPONSIBLE FOR INNER WELDED RIB DEFECTS ON SMALL AND MEDIUM-SIZED STRAIGHT-SEAM WELDED STEEL PIPES AND RELEVANT COUNTER-MEASURES

    • 摘要: 分析了中小直缝焊管生产存在的内焊筋缺陷成因,通过改进孔型设计、成型工艺、焊接工艺及提高管坯质量可有效地防止该缺陷的产生。

       

      Abstract: The elements responsible for inner welded rib defects existing on small and medium-sized straight-seam welded steel pipes are analyzed, based on which it is concluded that such defects can be prevented effectively by improving pass design, forming technology, welding technology and strip quality.

       

    /