φ108三辊穿孔机轧辊断轴原因分析
AN APPROACH TO ROLL SHAFT FRACTURE IN RESPECT TO Ф108mm THREE-ROLL PIERCING MILL
-
摘要: 分析了三辊穿孔机轧辊断轴的原因。在不改变穿孔机机架的条件下,对轧辊轴的危险断面尺寸、热处理工艺等进行了试验。40Cr钢轧辊轴只要设计和热处理合理,完全可以适应生产要求。Abstract: The article gives analyses concerning roll shaft fracture happening on the three-roll piercing mill. Based on the experiments on such aspects as dimensions of the shaft critical section, shaft heat-treatment process, etc., which were made without changing the mill housing. It is concluded that the 40Cr steel made roll shaft can completely meet the requirements of normal production provided that it is designed and heat-treated properly.