第三代核电主管道的制造技术

    Manufacturing Technology of The Third Generation Nuclear Power Reactor Coolant Pipe

    • 摘要: 介绍了国内外核电主管道制造技术的发展;指出目前国内制造第三代核电主管道的方法是采用实心电渣重熔坯锻造,再通过机加工掏空方式成型主管道的内孔;针对主管道制造传统工艺存在材料利用率低、生产周期长以及质量不稳定等特点,探讨了工艺改进的方向。分析认为:以离心铸造空心锭或电渣重熔空心锭为坯料的空心锻造工艺将最终替代目前的实心锻造工艺。

       

      Abstract: Described in the essay is the developments concerning the manufacture technologies for the nuclear power reactor coolant pipe as made both at home and abroad.It is pointed out that at present the process as used at home for making the third generation coolant pipe is first forging the solid electroslag remelting ingot,and then boring the shaped piece with mechanical method.Addressing the disadvantages concerning the conventional manufacturing process for the coolant pipe,i.e.,poor material utilization rate,rather long production cycle and product quality inconsistency,etc.,the orientation of technological improvement is discussed.The result of relevant analysis leads to such a forecast that the hollow forging process using the centrifugally-cast hollow ingot or the electroslag remelting hollow ingot as the blank will eventually replace the currently-employed solid billet forging process.

       

    /

    返回文章
    返回