TIAN Xiangyuan, YAN Anqing, YAO Yong, JI Ling. Cause Analysis for Surface Defect of L80-1 Oil Casing and Relevant Corrective Measures[J]. STEEL PIPE, 2022, 51(2): 47-49. DOI: 10.19938/j.steelpipe.1001-2311.2022.2.47.49
    Citation: TIAN Xiangyuan, YAN Anqing, YAO Yong, JI Ling. Cause Analysis for Surface Defect of L80-1 Oil Casing and Relevant Corrective Measures[J]. STEEL PIPE, 2022, 51(2): 47-49. DOI: 10.19938/j.steelpipe.1001-2311.2022.2.47.49

    Cause Analysis for Surface Defect of L80-1 Oil Casing and Relevant Corrective Measures

    • Addressing several types of defects with crack characteristics as occurring during the production process of the L80-1 oil casing,the material and manufacturing process of the said casing are described,and the macro and micro morphologies of three defects are analyzed.Furthermore based on the on-the-site statuses of hot-rolling,heat treatment and non-destructive detection operations,the possible reasons for the said defects are deduced,and accordingly corrective measures are taken to get the defect occurrence properly controlled.
    • loading

    Catalog

      Turn off MathJax
      Article Contents

      /

      DownLoad:  Full-Size Img  PowerPoint
      Return
      Return