ZHANG Guokuan, TIAN Xiaoyan. Causes for and Eliminating of Inner Surface Spiral-line Marks of Steel Pipes as Made with Two Different Types of Piercing Mills[J]. STEEL PIPE, 2015, 44(2): 51-54.
    Citation: ZHANG Guokuan, TIAN Xiaoyan. Causes for and Eliminating of Inner Surface Spiral-line Marks of Steel Pipes as Made with Two Different Types of Piercing Mills[J]. STEEL PIPE, 2015, 44(2): 51-54.

    Causes for and Eliminating of Inner Surface Spiral-line Marks of Steel Pipes as Made with Two Different Types of Piercing Mills

    • It is commonly encountered with that defective inner spiral-line marks occur with seamless steel tubes being hot-rolled by either of the two typical piercing mills,i.e.,the barrel type rotary piercer and the cone type piercer.Causes for the said defect are investigated in terms of deformation zone and cold(thermal) rolling tools,and eventually identified.Accordingly,preventative measures are proposed,including adding one more cross-rolling stand,reducing the roll face angle of the roll outlet cone part,correctly selecting cold(thermal) rolling tolls,and preventing interference of any external element,etc.
    • loading

    Catalog

      Turn off MathJax
      Article Contents

      /

      DownLoad:  Full-Size Img  PowerPoint
      Return
      Return