Deng Pian, Zhou Mengxiong. Investigation of Causes Responsible for Wall Thickness Tolerance of Shell as Hot-rolled with Semi-floating Mandrel Mill[J]. STEEL PIPE, 2005, 34(5): 18-22.
    Citation: Deng Pian, Zhou Mengxiong. Investigation of Causes Responsible for Wall Thickness Tolerance of Shell as Hot-rolled with Semi-floating Mandrel Mill[J]. STEEL PIPE, 2005, 34(5): 18-22.

    Investigation of Causes Responsible for Wall Thickness Tolerance of Shell as Hot-rolled with Semi-floating Mandrel Mill

    More Information
    • Received Date: November 21, 2004
    • Revised Date: April 07, 2005
    • Available Online: December 14, 2023
    • As for wall thickness unevenness of the shell produced with the semi-floating mandrel mill,there could be such different types as batch wall thickness unevenness,shall longitudinal wall thickness unevenness and transversal wall thickness unevenness.The causes for shell wall thickness unevenness are identified.Transversal wall thickness unevenness is due to the original wall thickness unevenness of the pierced hollow bloom,some change of the mandrel mill roll groove and deviation of the rolling centerline,while longitudinal wall thickness unevenness and batch wall thickness unevenness are due to geometric inconsistency of the mandrel.Countermeasures are proposed,accordingly.

    Catalog

      Article views (7) PDF downloads (6) Cited by()
      Turn off MathJax
      Article Contents

      /

      DownLoad:  Full-Size Img  PowerPoint
      Return
      Return